For PE Coextruded (aged), surface energy (dyne/cm) is 32–38; condition is Migration; needs treatment? is Often, verified against its source on 2026-08-04.

- **Material:** PE Coextruded (aged)
- **Surface energy (dyne/cm):** 32–38
- **Condition:** Migration
- **Needs treatment?:** Often

## What the source says

> PE Coextruded (aged) | 32–38 | Migration | Often | Dyne pens | Surface energy loss over time |