PE Film

For PE Film, surface energy (dyne/cm) is 30–33; condition is Untreated; needs treatment? is Yes, verified against its source on 2026-08-04.

Material
PE Film
Surface energy (dyne/cm)
30–33
Condition
Untreated
Needs treatment?
Yes
Sourcekolorguide.com
Verified2026-08-04
Review by2028-08-03
DatasetGalvanic series and surface energy of engineering materials

What the source says

PE Film | 30–33 | Untreated | Yes | Dyne pens | Requires treatment |

kolorguide.com, retrieved 2026-08-04