Reference Source

PE Coextruded (treated)

For PE Coextruded (treated), surface energy (dyne/cm) is 38–42; condition is Corona treated; needs treatment? is No, verified against its source on 2026-08-04.

Material
PE Coextruded (treated)
Surface energy (dyne/cm)
38–42
Condition
Corona treated
Needs treatment?
No
Sourcekolorguide.com
Verified2026-08-04
Review by2028-08-03
DatasetGalvanic series and surface energy of engineering materials

What the source says

PE Coextruded (treated) | 38–42 | Corona treated | No | Dyne pens | Printable surface |

kolorguide.com, retrieved 2026-08-04

Source