PE Coextruded (aged)
For PE Coextruded (aged), surface energy (dyne/cm) is 32–38; condition is Migration; needs treatment? is Often, verified against its source on 2026-08-04.
- Material
- PE Coextruded (aged)
- Surface energy (dyne/cm)
- 32–38
- Condition
- Migration
- Needs treatment?
- Often
What the source says
PE Coextruded (aged) | 32–38 | Migration | Often | Dyne pens | Surface energy loss over time |
— kolorguide.com, retrieved 2026-08-04
Source
- kolorguide.comhttps://kolorguide.com/surface-energy-chart-by-material/